Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Flint Hills AP6835-HS Polypropylene Impact Copolymer Features: Excellent processing, good low temperature impact strength.Applications: Injection molding: Appliance components, consumer durables and closuresInformation Provided by Flint Hills Resource.. |
|||
Gardner Impact | >= 36.0 J @Temperature -30.0 °C |
>= 26.6 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
Flint Hills AP7710-HS Impact Copolymer Polypropylene TPO copolymer, UL certified, and FDA compliant.Features: Structural stiffness, ultra high impact strength, and high uniform flow rate.Applications: Injection molding: automotive items and exterior e.. |
|||
Gardner Impact | >= 36.0 J | >= 26.6 ft-lb | ASTM D3029 |
Flint Hills P5M4K-046 Random Copolymer Polypropylene Random copolymer, FDA compliant.Features: Clarified (50 mil plaque haze 10%), antistat, and controlled rheology.Applications: Injection molding: high clarity parts, medical parts, and good organolep.. |
|||
Gardner Impact | 36.0 J | 26.6 ft-lb | ASTM D3029 |
LyondellBasell Astryn SB572C Polypropylene Copolymer Key Features: fractional melt flow, medium modulus, extrusion grade polypropylene copolymer, good melt strength, good processabilityApplications: solar panelsDescription: Astryn SB572C fractional me.. |
|||
Gardner Impact | 36.0 J | 26.6 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1000F PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 Listing. Effective June, 2007 this grade will no long.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Gardner Impact | >= 36.0 J | >= 26.6 ft-lb | |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Gardner Impact | >= 36.0 J | >= 26.6 ft-lb | |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Gardner Impact | >= 36.0 J | >= 26.6 ft-lb | |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Gardner Impact | 36.0 J | 26.6 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in natural color. Effective June, 20.. |
|||
Gardner Impact | 36.0 J | 26.6 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer.. |