Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 33.0 J @Thickness 3.17 mm |
24.3 ft-lb @Thickness 0.125 in |
|
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA) High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren.. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
LyondellBasell Astryn BA35H Polypropylene Copolymer, Flame Retardant Key Features: conventional melt flow, medium modulus, flame retardant polypropylene copolymer, UL 94 V-2 flames, good electrical properties and insulating characteristics, good aesthetics and colora.. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1010F PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1010F PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1010M PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1010P PEI Enhanced flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1010R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1010R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM HU1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Gardner Impact | 33.0 J @Temperature 23.0 °C |
24.3 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Noryl PX1404 PPE+PS PPE+PS blend. High Heat. FDA compliant with restrictions. Injection Molding and Extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
Gardner Impact | 33.0 J @Temperature -40.0 °C |
24.3 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
SABIC Innovative Plastics NORYL BN31 PPE+PS Blowmoldable. Excellent processability and flammability. Good heat resistance. Low temperature impact strength. Dimensional stability. |
|||
Gardner Impact | 33.0 J | 24.3 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 1010M PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |