Polymer Property : Gardner Impact = 17.50 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 23.73 J
17.50 ft-lb
ASTM D3029
Multibase Multi-Flam™ 1502 PP Black Polypropylene
Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase