Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Multibase Multi-Flex® TPE D 4510 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 5002 CU Natural 50% Filler Content Polypropylene This product is well suited for non-glossy appliance type parts. It replaces ABS at favorable cost performance characteristics and can be made UV stable. This product can be color matched in most c.. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT1001-74 Thermoplastic Polyolefin, Non-UV Stabilized, DX9 Black Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT2700-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT4650-581UV Thermoplastic Polyolefin, UV Stabilized, HD2 Medium Quartz Metallic Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products HP521-188 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9777 Medium Beige Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P250-01 Polypropylene Copolymer, Black Applications: ConsolesConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P251-00 Polypropylene Copolymer, Natural Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P252-01 Polypropylene Copolymer, Black Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P256-00 Polypropylene Copolymer, Natural Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P256-01 Polypropylene Copolymer, Black Applications: Door/trunk scuffConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J @Temperature -18.0 °C |
16.7 ft-lb @Temperature -0.400 °F |
|
Network Polymers NPP 25-1002 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Gardner Impact | 22.6 J @Temperature -18.0 °C |
16.7 ft-lb @Temperature -0.400 °F |
Gardner |
Network Polymers NPP 25-2002 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Gardner Impact | 22.6 J @Temperature -30.0 °C |
16.7 ft-lb @Temperature -22.0 °F |
Method G, geometry GC; ASTM D5420 |
Pinnacle Polymers 3208 High Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Gardner Impact | 22.6 J @Temperature -30.0 °C |
16.7 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J @Temperature -30.0 °C |
16.7 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J @Temperature 23.0 °C |
16.7 ft-lb @Temperature 73.4 °F |
ASTM D3029 |
ExxonMobil Paxon™ BA7718 Sheet Extrusion and Blow Molding Resin
(discontinued **) BA7718 is a 25% brown mica-filled, medium molecular weight, high density polyethylene. This material has been specifically developed as a cost effective resin for applications which require outstan.. |