Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | >= 190 J | >= 140 ft-lb | ASTM D5420 |
Buckeye Polymers BP RPPC 2010 CW Polypropylene, Calcium Filled Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges fro.. |
|||
Gardner Impact | >= 190 J | >= 140 ft-lb | ASTM D5420 |
Buckeye Polymers BP FLEX D5518 R 848 Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |