Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 17.5 J | 12.9 ft-lb | ASTM D5420 |
RheTech Products FT3150-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsUnderhood componentsBumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |