Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 15.02 J @Thickness 3.20 mm, Temperature -30.0 °C |
11.08 ft-lb @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D3029 |
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman. |
|||
Gardner Impact | 15.02 J | 11.08 ft-lb | ASTM D3029 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Gardner Impact | 15.02 J @Thickness 3.20 mm, Temperature -30.0 °C |
11.08 ft-lb @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D3029 |
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman. |
|||
Gardner Impact | 15.02 J | 11.08 ft-lb | ASTM D3029 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Gardner Impact | 15.02 J @Thickness 3.20 mm, Temperature -30.0 °C |
11.08 ft-lb @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D3029 |
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman. |
|||
Gardner Impact | 15.02 J | 11.08 ft-lb | ASTM D3029 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Gardner Impact | 15.02 J @Thickness 3.20 mm, Temperature -30.0 °C |
11.08 ft-lb @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D3029 |
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman. |
|||
Gardner Impact | 15.02 J | 11.08 ft-lb | ASTM D3029 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Gardner Impact | 15.02 J @Thickness 3.20 mm, Temperature -30.0 °C |
11.08 ft-lb @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D3029 |
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman. |
|||
Gardner Impact | 15.02 J | 11.08 ft-lb | ASTM D3029 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Gardner Impact | 15.02 J | 11.08 ft-lb | ASTM D3029 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Gardner Impact | 15.02 J @Thickness 3.20 mm, Temperature -30.0 °C |
11.08 ft-lb @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D3029 |
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman. |