Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 2.30 J | 1.70 ft-lb | ASTM D3029 |
Washington Penn PPH2UFO Polypropylene, Unfilled Homopolymer for injection molding. Meets General Motors spec. GMP.PP.013Data provided by Washington Penn Plastic Co., Inc. |
|||
Gardner Impact | 2.30 J | 1.70 ft-lb | ASTM D3029 |
Adell RA-16 Copolymer Polypropylene, 30% Talc Filled Data provided by Adell Plastics, Inc. |