Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products FRG220-773UB 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Flame Retardant, UV Stabilized, Light Grey Applications: Electrical housingsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products G13P100-01 13% Glass Fiber Reinforced Polypropylene, Black Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products G13P100-01UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products GC20P200-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsBoat handlesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products GC20P255-01UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Durable goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products T15P100-00 12% Talc Reinforced Polypropylene, Natural Applications: Component housingConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products T30P100-00 30% Talc Reinforced Polypropylene, Natural Applications: Headlamp housingsI/P componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products T30P100-01 30% Talc Reinforced Polypropylene, Black Applications: BracketsAir ductsConsolesWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products GC20P255-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: BracketsUnderhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.790 J | 0.583 ft-lb | ASTM D5420 |
RheTech Products GC20P255-712UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, B231 Earth Grey Applications: Consumer goodsMiscellaneous bracketsExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |