Polymer Property : Gardner Impact = 6.30 J
Polymer Property :
Gardner Impact =
6.30 J
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Gardner Impact
6.30
J
4.65
ft-lb
ASTM D3029 GB
Plaskolite West Optix® CA-1000 E Impact Modified Acrylic Resin
Extrusion Grade Pellets. Excellent blend stock material for impact applications.