Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | >= 35.0 J @Temperature -30.0 °C |
>= 25.8 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
Flint Hills AP7310-HS Impact Copolymer Polypropylene Ultra high impact copolymer, UL certified, and FDA compliant.Features: Heat stabilized.Applications: Injection molding: appliance components, automotive exterior and underbody components, constructi.. |
|||
Gardner Impact | 35.0 J | 25.8 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 9075 PEI High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Gardner Impact | 35.0 J | 25.8 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 9075 PEI (Asia Pacific) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Gardner Impact | 35.0 J | 25.8 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 9076 PEI Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Gardner Impact | 35.0 J | 25.8 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Gardner Impact | 35.0 J @Temperature 23.0 °C |
25.8 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Gardner Impact | 35.0 J | 25.8 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM LTX300B PEI Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
Gardner Impact | 35.0 J | 25.8 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific) Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
Gardner Impact | 35.0 J | 25.8 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Gardner Impact | 35.0 J | 25.8 ft-lb | ASTM D3029 |
SABIC Innovative Plastics ULTEM 9076 PEI (Asia Pacific) Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |