Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT1001-74 Thermoplastic Polyolefin, Non-UV Stabilized, DX9 Black Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT1003-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step and hitch padsInterior component and trimA/B pillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT2600-677UV Thermoplastic Polyolefin, UV Stabilized, 0848 Black Applications: Exterior trimStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT4650-581UV Thermoplastic Polyolefin, UV Stabilized, HD2 Medium Quartz Metallic Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P250-01 Polypropylene Copolymer, Black Applications: ConsolesConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P251-00 Polypropylene Copolymer, Natural Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P254-00 Polypropylene Copolymer, Natural Applications: Air ducts - distributionInterior trimI/P componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P254-01 Polypropylene Copolymer, Black Applications: Air ducts - distributionFuse panel coversSplash shieldsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P256-00 Polypropylene Copolymer, Natural Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products P256-01A Polypropylene Copolymer, Black Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J @Temperature -30.0 °C |
16.7 ft-lb @Temperature -22.0 °F |
Gardner |
Network Polymers NPP 25-0803 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Gardner Impact | 22.6 J @Temperature -18.0 °C |
16.7 ft-lb @Temperature -0.400 °F |
|
Network Polymers NPP 25-2003 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products HP521-288UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167A Ebony Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products HP522-286 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZUCA Medium Graphite Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D3029 |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J @Temperature -30.0 °C |
16.7 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 22.6 J | >= 16.7 ft-lb | ASTM D3029 |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 22.6 J | 16.7 ft-lb | ASTM D5420 |
RheTech Products E204-00 High Density Polyethylene, Natural Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |