Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D5420 |
RheTech Products CC20P200-00 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Natural Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D5420 |
RheTech Products FT4200-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D5420 |
RheTech Products FT4200-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D3029 |
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan.. |
|||
Gardner Impact | 13.6 - 16.9 J | 10.0 - 12.5 ft-lb | Average value: 16.3 J Grade Count:15 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Gardner Impact | 13.6 J @Temperature 22.8 °C |
10.0 ft-lb @Temperature 73.0 °F |
ASTM D5420 |
Spartech PP7140 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D5420 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D5420 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D5420 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J @Temperature 23.0 °C |
10.0 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Homopolymer Polypropylene 10% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D5420 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D5420 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D5420 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D3029 |
Adell RZ-14 Copolymer Polypropylene, 20% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D5420 |
RheTech Products CC20P200-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |