Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 1.36 J | 1.00 ft-lb | ASTM D5420 |
RheTech Products T20P100-01EG 20% Talc Reinforced Polypropylene, General Purpose Black, Extrusion Grade Applications: Consumer goodsAutomotive componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.36 J @Temperature 22.8 °C |
1.00 ft-lb @Temperature 73.0 °F |
ASTM D5420 |
Spartech PP5120 Talc Filled Homopolymer Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech |
|||
Gardner Impact | >= 1.36 J @Temperature 22.8 °C |
>= 1.00 ft-lb @Temperature 73.0 °F |
ASTM D5420 |
Spartech PP5130 Talc Filled Homopolymer Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech |
|||
Gardner Impact | >= 1.36 J @Temperature 22.8 °C |
>= 1.00 ft-lb @Temperature 73.0 °F |
ASTM D5420 |
Spartech PP5140 Talc Filled Homopolymer Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech |
|||
Gardner Impact | 1.36 J | 1.00 ft-lb | ASTM D3029 |
Plastics Group Polifil® GFRMPPCC-10 10% Glass Reinforced Polypropylene, High Impact Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap.. |