Polymer Property : Gardner Impact = 1.35582 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 1.35582 - 43.3862 J

@Temperature -30.0 - -5.56 °C
1.00000 - 32.0000 ft-lb

@Temperature -22.0 - 22.0 °F
Average value: 13.7 J Grade Count:4
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Gardner Impact 1.35582 - 1.35582 J

@Temperature -30.0 - -5.56 °C
1.00000 - 1.00000 ft-lb

@Temperature -22.0 - 22.0 °F
Average value: 3.11 J Grade Count:2
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..