Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 1.02 J | 0.750 ft-lb | ASTM D5420 |
RheTech Products GC15P200-00 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.02 J | 0.750 ft-lb | ASTM D5420 |
RheTech Products P100-00 Polypropylene, Natural Applications: Automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.02 J | 0.750 ft-lb | ASTM D5420 |
RheTech Products P100-01 Polypropylene Homopolymer, Black Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.02 J | 0.750 ft-lb | ASTM D5420 |
RheTech Products P102-00 Polypropylene, Black Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.02 J | 0.750 ft-lb | ASTM D5420 |
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.02 J | 0.750 ft-lb | ASTM D5420 |
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.02 J | 0.750 ft-lb | ASTM D5420 |
RheTech Products GC20P600-01UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black Applications: Sun roof trimFan shroudInjection molding conditions reported in table.Information provided by RheTech Products. |