Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 0.294 J @Temperature 23.0 °C |
0.217 ft-lb @Temperature 73.4 °F |
per mil, 1/2" R Tup |
Axiall HH-2000 Rigid PVC, Molding Georgia Gulf HH-2000 is a high heat/high flow injection molding grade PVC alloy with a price/performance niche between high flow vinyl and utility engineering thermoplastics. It combines excellent .. |