Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 570 J/cm | 1.07 ft-lb/mil | Puncture Resistance; SABIC Method |
SABIC 318B Linear Low Density Polyethylene for Cast Film Product Description: 318B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Dart Drop Total Energy | 570 - 890 J/cm | 1.07 - 1.67 ft-lb/mil | Average value: 656 J/cm Grade Count:7 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |