Polymer Property : Dart Drop Total Energy = 0.450 ft-lb/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Total Energy 240 J/cm
0.450 ft-lb/mil
DIN 53373
BASF Ecovio® C2332 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2332 is our biodegradable film product containing 18% renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic..