Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 46.7 - 161 J/cm | 0.0875 - 0.302 ft-lb/mil | Average value: 85.5 J/cm Grade Count:4 |
Overview of materials for PVC, Sheet Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |