Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.01231 GPa | 1.785 ksi | |
TSE Industries Millathane® 66 Millable Polyurethane Rubber Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical .. |
|||
200% Modulus | 0.01231 GPa | 1.785 ksi | |
TSE Industries Millathane® 66 Millable Polyurethane Rubber Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical .. |