Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00498 GPa | 0.723 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-550 (FEF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00498 GPa | 0.723 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-774 (SRF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00498 GPa | 0.723 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00498 GPa | 0.723 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-550 (FEF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00498 GPa | 0.723 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-774 (SRF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00498 GPa | 0.723 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |