Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 3.20 J/cm² | 15.2 ft-lb/in² | ASTM D256 |
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Izod Impact Resistance | 3.20 J/cm² | 15.2 ft-lb/in² | |
Dow HDPE 30460M High Density Polyethylene DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent pro.. |