Polymer Property : Puncture Energy = 57.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 57.0 J

@Temperature -40.0 °C
42.0 ft-lb

@Temperature -40.0 °F
Energy @ Max. Load; ASTM D3763
Eastman Tritan LX150HF Copolyester
Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades ..