Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 31.0 J @Thickness 3.20 mm, Temperature 23.0 °C |
22.9 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
max load; ASTM D3763 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Puncture Energy | 31.0 J @Thickness 2.70 mm, Temperature 23.0 °C |
22.9 ft-lb @Thickness 0.106 in, Temperature 73.4 °F |
max load; ASTM D3763 |
Eastman 9921P PET Injection Molded
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Puncture Energy | 31.0 J @Thickness 3.20 mm, Temperature 23.0 °C |
22.9 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
max load; ASTM D3763 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Puncture Energy | 31.0 J @Thickness 3.20 mm, Temperature 23.0 °C |
22.9 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
max load; ASTM D3763 |
Eastman Eastar MN021 Copolyester Eastar copolyester MN021 is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Puncture Energy | 31.0 J @Thickness 3.20 mm, Temperature 23.0 °C |
22.9 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
max load; ASTM D3763 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |