Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 2.10 J @Thickness 3.20 mm, Temperature -40.0 °C |
1.55 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
max load; ASTM D3763 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Puncture Energy | 2.10 J @Temperature -30.0 °C |
1.55 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Puncture Energy | 2.10 J @Thickness 3.20 mm, Temperature -40.0 °C |
1.55 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
max load; ASTM D3763 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Puncture Energy | 2.10 J @Thickness 3.20 mm, Temperature -40.0 °C |
1.55 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
max load; ASTM D3763 |
Eastman Eastar MN021 Copolyester Eastar copolyester MN021 is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Puncture Energy | 2.10 J @Thickness 3.20 mm, Temperature -40.0 °C |
1.55 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
max load; ASTM D3763 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |