Polymer Property : Puncture Energy = 15.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 15.0 J

@Thickness 2.50 mm,
Temperature 23.0 °C
11.1 ft-lb

@Thickness 0.0984 in,
Temperature 73.4 °F
max load; ISO 6603-2
Eastman 9921 PET Injection Molded  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Puncture Energy 15.0 J

@Temperature -20.0 °C
11.1 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Borealis BD950MO Polypropylene Copolymer
BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability..
Puncture Energy 15.0 J

@Thickness 2.50 mm,
Temperature 23.0 °C
11.1 ft-lb

@Thickness 0.0984 in,
Temperature 73.4 °F
max load; ISO 6603-2
Eastman Eastar EN001 Copolyester
Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro..
Puncture Energy 15.0 J

@Thickness 2.50 mm,
Temperature 23.0 °C
11.1 ft-lb

@Thickness 0.0984 in,
Temperature 73.4 °F
max load; ISO 6603-2
Eastman 9921W PET Injection Molded  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..