Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.00 J @Thickness 3.20 mm, Temperature -40.0 °C |
0.738 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
max load; ISO 6603-2 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Puncture Energy | 1.00 J @Thickness 3.20 mm, Temperature -40.0 °C |
0.738 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
max load; ISO 6603-2 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Puncture Energy | 1.00 J @Thickness 3.20 mm, Temperature -40.0 °C |
0.738 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
max load; ISO 6603-2 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |