Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.64 GPa @Strain 0.450 %, Temperature 40.0 °C |
529 ksi @Strain 0.450 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Secant Modulus | 3.65 GPa @Strain 1.00 %, Temperature -40.0 °C |
529 ksi @Strain 1.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |