Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.42 GPa @Strain 0.250 %, Temperature 40.0 °C |
496 ksi @Strain 0.250 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Secant Modulus | 3.42 GPa @Strain 0.290 %, Temperature 23.0 °C |
496 ksi @Strain 0.290 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Secant Modulus | 3.42 GPa @Strain 0.290 %, Temperature 23.0 °C |
496 ksi @Strain 0.290 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |
|||
Secant Modulus | 3.42 GPa @Strain 1.50 %, Temperature 80.0 °C |
496 ksi @Strain 1.50 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Secant Modulus | 3.42 GPa @Strain 3.60 %, Temperature 40.0 °C |
496 ksi @Strain 3.60 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |