Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.56 GPa @Strain 3.16 %, Temperature 40.0 °C |
371 ksi @Strain 3.16 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)