Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.39 GPa @Strain 2.00 %, Temperature 23.0 °C |
346 ksi @Strain 2.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |
|||
Secant Modulus | 2.39 GPa @Strain 1.50 %, Temperature 100 °C |
346 ksi @Strain 1.50 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |