Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.05 GPa @Strain 0.230 %, Temperature 0.000 °C |
298 ksi @Strain 0.230 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |
|||
Secant Modulus | 2.06 GPa @Strain 2.00926 %, Temperature 80.0 °C |
298 ksi @Strain 2.00926 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |