Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.187 GPa @Strain 11.06 %, Temperature 40.0 °C |
27.1 ksi @Strain 11.06 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |
|||
Secant Modulus | 0.187 GPa @Strain 29.6 %, Temperature -20.0 °C |
27.1 ksi @Strain 29.6 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |