Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.75 GPa @Strain 2.40 %, Temperature 23.0 °C |
254 ksi @Strain 2.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Secant Modulus | 1.75 GPa @Strain 2.40 %, Temperature 23.0 °C |
254 ksi @Strain 2.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Secant Modulus | 1.75 GPa @Strain 2.63 %, Temperature 200 °C |
254 ksi @Strain 2.63 %, Temperature 392 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G35EF BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN51G35EF BK083 is a 35% glass reinforced heat stabilized lubricated high performance.. |
|||
Secant Modulus | 1.75 GPa @Strain 2.63 %, Temperature 200 °C |
254 ksi @Strain 2.63 %, Temperature 392 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Secant Modulus | 1.75 GPa @Strain 4.24 %, Temperature 0.000 °C |
254 ksi @Strain 4.24 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |