Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.14 GPa @Temperature 200 °C |
165 ksi @Temperature 392 °F |
ASTM D882 |
DuPont™ Kapton® 150FN019 Polyimide/FEP Composite Film 150 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r.. |
|||
Secant Modulus | 1.14 GPa @Strain 2.20 %, Temperature 100 °C |
165 ksi @Strain 2.20 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |