Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 9.21 GPa @Strain 1.20 %, Temperature 23.0 °C |
1340 ksi @Strain 1.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol.. |
|||
Secant Modulus | 9.23 GPa @Strain 1.30 %, Temperature 0.000 °C |
1340 ksi @Strain 1.30 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol.. |
|||
Secant Modulus | 9.25 GPa @Strain 2.70 %, Temperature -40.0 °C |
1340 ksi @Strain 2.70 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |
|||
Secant Modulus | 9.21 GPa @Strain 1.20 %, Temperature 23.0 °C |
1340 ksi @Strain 1.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo.. |
|||
Secant Modulus | 9.23 GPa @Strain 1.30 %, Temperature 0.000 °C |
1340 ksi @Strain 1.30 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo.. |
|||
Secant Modulus | 9.21 GPa @Strain 0.786074 %, Temperature 23.0 °C |
1340 ksi @Strain 0.786074 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |