Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 8.87 GPa @Strain 0.950 %, Temperature 23.0 °C |
1290 ksi @Strain 0.950 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Secant Modulus | 8.90 GPa @Strain 1.23431 %, Temperature 0.000 °C |
1290 ksi @Strain 1.23431 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |