Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 8.57 GPa @Strain 1.485 %, Temperature 0.000 °C |
1240 ksi @Strain 1.485 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Secant Modulus | 8.57 GPa @Strain 0.700 %, Temperature 40.0 °C |
1240 ksi @Strain 0.700 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol.. |
|||
Secant Modulus | 8.57 GPa @Strain 0.700 %, Temperature 40.0 °C |
1240 ksi @Strain 0.700 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo.. |
|||
Secant Modulus | 8.55 GPa @Strain 2.01539 %, Temperature -40.0 °C |
1240 ksi @Strain 2.01539 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |