Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 8.00 GPa @Strain 0.250 %, Temperature 23.0 °C |
1160 ksi @Strain 0.250 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Secant Modulus | 8.00 GPa @Strain 1.55 %, Temperature 0.000 °C |
1160 ksi @Strain 1.55 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |
|||
Secant Modulus | 8.02 GPa @Strain 0.210062 %, Temperature 40.0 °C |
1160 ksi @Strain 0.210062 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |