Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 7.50 GPa @Strain 1.77 %, Temperature 0.000 °C |
1090 ksi @Strain 1.77 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Secant Modulus | 7.51 GPa @Strain 2.00 %, Temperature 23.0 °C |
1090 ksi @Strain 2.00 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) 43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information.. |
|||
Secant Modulus | 7.50 GPa @Strain 0.680 %, Temperature 23.0 °C |
1090 ksi @Strain 0.680 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |