Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.62 - 10.2 GPa @Temperature -40.0 - 100 °C |
235 - 1480 ksi @Temperature -40.0 - 212 °F |
Average value: 5.73 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Secant Modulus | 1.62 - 10.2 GPa @Strain 0.250 - 3.50 % |
235 - 1480 ksi @Strain 0.250 - 3.50 % |
Average value: 5.73 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |