Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 8.15 GPa @Strain 0.520 %, Temperature 40.0 °C |
1180 ksi @Strain 0.520 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |