Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 7.62 GPa @Strain 0.453157 %, Temperature 40.0 °C |
1100 ksi @Strain 0.453157 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |