Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 4.65654 - 8.95349 GPa @Temperature -20.0 - 40.0 °C |
675.385 - 1298.61 ksi @Temperature -4.00 - 104 °F |
Average value: 7.36 GPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Secant Modulus | 4.65654 - 8.95349 GPa @Strain 0.520 - 2.83 % |
675.385 - 1298.61 ksi @Strain 0.520 - 2.83 % |
Average value: 7.36 GPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |