Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.85 GPa @Strain 1.50 %, Temperature 100 °C |
413 ksi @Strain 1.50 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Secant Modulus | 2.85 GPa @Strain 3.14 %, Temperature 100 °C |
414 ksi @Strain 3.14 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Secant Modulus | 2.85 GPa @Strain 1.10 %, Temperature 23.0 °C |
413 ksi @Strain 1.10 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |