Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.48 GPa @Strain 1.59 %, Temperature 23.0 °C |
359 ksi @Strain 1.59 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Secant Modulus | 2.48 GPa @Temperature 23.0 °C |
360 ksi @Temperature 73.4 °F |
ASTM D882 |
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film 120 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 2.5 µm (0.1 mil) coating of Teflon® FEP on both sides.Kapton® Type HN film coated with Teflon® FEP fluoropolyme.. |