Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.24 GPa @Strain 0.190 %, Temperature -20.0 °C |
325 ksi @Strain 0.190 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |