Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.17 GPa @Strain 2.40 %, Temperature 0.000 °C |
314 ksi @Strain 2.40 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Secant Modulus | 2.17 GPa @Strain 1.71 %, Temperature 40.0 °C |
314 ksi @Strain 1.71 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Secant Modulus | 2.17 GPa @Strain 3.70 %, Temperature -40.0 °C |
315 ksi @Strain 3.70 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro.. |
|||
Secant Modulus | 2.17 GPa @Strain 2.40 %, Temperature 0.000 °C |
314 ksi @Strain 2.40 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Secant Modulus | 2.17 GPa @Strain 1.71 %, Temperature 40.0 °C |
314 ksi @Strain 1.71 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |
|||
Secant Modulus | 2.17 GPa @Strain 1.92 %, Temperature 40.0 °C |
314 ksi @Strain 1.92 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |