Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.06 GPa @Strain 4.00 %, Temperature 100 °C |
299 ksi @Strain 4.00 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |
|||
Secant Modulus | 2.06 GPa @Strain 3.17 %, Temperature -40.0 °C |
299 ksi @Strain 3.17 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien.. |
|||
Secant Modulus | 2.06 GPa @Strain 0.250 %, Temperature 100 °C |
299 ksi @Strain 0.250 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 2.06 GPa @Strain 2.00926 %, Temperature 80.0 °C |
298 ksi @Strain 2.00926 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |